Steel grades - Sheet piles
Hot rolled sections (except GU sections)
Mechanical properties according to EN 10248-1:1995 and comparable international standards. Other steel grades can be delivered on request.
| Standard referred to: EN 10248-1:1995 |
Comparable international standards |
Steel grade |
Minimum yield strength ReH |
Minimum tensile strength Rm |
Minimum elongation
 |
USA |
Canada |
Japan |
| N/mm2 |
N/mm2 |
% |
ASTM |
CSA G 4021 |
JIS A 5528 |
| S 240 GP |
240 |
340 |
26 |
|
|
|
| S 270 GP |
270 |
410 |
24 |
A 328 |
Gr. 260 W |
|
| S 320 GP |
320 |
440 |
23 |
|
Gr. 300 W |
|
| S 355 GP |
355 |
480 |
22 |
A 572 Gr. 50; A 690 |
Gr. 350 W |
|
| S 390 GP |
390 |
490 |
20 |
A 572 Gr. 55 |
|
SY 390 |
| S 430 GP |
430 |
510 |
19 |
A 572 Gr. 60 |
Gr. 400 W |
|
| ArcelorMittal Mill Specification |
|
| S 460 AP |
460 |
550 |
17 |
A 572 Gr. 65 |
|
|
Grades S 460 AP, A 690 and A 572 Gr. 65 on request.
Hot rolled GU sections
Mechanical properties according to EN 10248-1:1995 and comparable international standards.
| Standard referred to: EN 10248-1:1995 |
Comparable international standards |
Steel grade |
Minimum yield strength ReH |
Minimum tensile strength Rm |
Minimum elongation
 |
USA |
Canada |
| N/mm2 |
N/mm2 |
% |
ASTM |
CSA G 4021 |
| S 240 GP |
240 |
340 |
26 |
|
|
| S 270 GP |
270 |
410 |
24 |
A 328 |
Gr. 260 W |
| S 320 GP |
320 |
440 |
23 |
|
Gr. 300 W |
| S 355 GP |
355 |
480 |
22 |
A 572 Gr. 50; A 690 |
Gr. 350 W |
Grade S 355 GP on request.
Cold formed sections
Mechanical properties according to EN 10249-1:1995 and corresponding former national standards. Other steel grades can be delivered on request.
| Standard referred to: EN 10249-1:1995 |
Former references |
Steel grade |
Minimum yield strength ReH |
Minimum Tensile strength Rm |
Minimum elongation
 |
F |
D |
GB |
B |
| N/mm2 |
N/mm2 |
% |
| S 235 JRC |
235 |
340-470 |
26 |
E 24-2 |
St 37.2 |
40 B |
AE 235-B |
| S 275 JRC |
275 |
410-560 |
22 |
E 28-2 |
St 44.2 |
43 B |
AE 275-B |
| S 355 JOC |
355 |
490-630 |
22 |
E 36-3 |
St 52.3 U |
50 C |
AE 355-C |
The C in JRC and J0C stands for cold forming aptitude according to EN 10025:1993.
|
|
|